Nickel Alloy N06044 - High-Performance Corrosion resistant alloy

Corrosion Resistant Alloy Series

N06044

Nickel Alloy N06044 is a high-chromium, austenitic nickel-chromium alloy with a controlled silicon content and rare earth additions.
The formation of a protective chromium oxide layer, together with a subjacent silicon oxide layer, makes the alloy especially suitable for applications such as waste incineration.

    CHEMICAL COMPOSITION

    ERAUM

    %

    Ni

    Cr

    Fe

    Mo

    Si

    C

    Mn

    S

    Al

    Ti

    P

    N06044

    MIN

    Rem

    43.5

    -

    0.80

    -

    -

    0.07

    -

    -

    -

    0.2

    MAX

    Rem

    45.3

    0.3

    1.20

    0.20

    0.02

    0.30

    0.35

    0.015

    0.3

    0.8

    Physical Properties

    density

    tensile strength

    yield strength

    Elongation

    Elongation

     7.98g/cm²

    Rm N/mm2

    Rp0.2 N/mm2

    A5%

    HRB

    Solid solution

    ≥690

    ≥310

    ≥30%

    ≤100

    EXECUTIVE STANDARD

    PRODUCT

    ASTM standard

    ASME standard

    Sheet, Plate, Strip

    B575

    SB575

    Seamless Pipe&tube

    B622

    -

    welded Pipe&tube

    -

    -

    Bar, Cake

    B574

    SB574

    Forging

    B564

    SB564

    Wire

    -

    -

    Product FEATURE

    1.N06044 has excellent mechanical properties, including high strength, high hardness, good toughness and fatigue resistance. 
    It has good corrosion resistance at room temperature and can withstand the erosion of many corrosive media such as acid, alkali and salt.Especially in strong acid, alkali and other harsh environments, its corrosion resistance is particularly outstanding.
    Antioxidant: The alloy can maintain stable antioxidant performance under high temperature and high pressure, and is not easy to oxidise and corrode.

    Product application

    Aerospace: Used in the manufacture of high-temperature burners, high-temperature steam pipes and other components.