0102030405
COMHRADH CHEMICAL
SPIORAD | % | c | Mn | Agus | Cr | S | Anns | Le | Fe | Al | As |
N08800 | MIN | - | - | - | 19 | - | 30 | - | cothromachadh | 0.15 | 0.15 |
MAX | 0.10 | 1.5 | 1 | 23 | 0.015 | 35 | 0.75 | cothromachadh | 0.60 | 0.60 | |
N08810 | MIN | 0.05 | - | - | 19 | - | 30 | - | cothromachadh | 0.15 | 0.15 |
MAX | 0.10 | 1.5 | 1 | 23 | 0.015 | 35 | 0.75 | cothromachadh | 0.60 | 0.60 | |
N08811 | MIN | 0.06 | - | - | 19 | - | 30 | - | cothromachadh | 0.15 | 0.15 |
MAX | 0.10 | 1.5 | 1 | 23 | 0.015 | 35 | 0.75 | cothromachadh | 0.60 | 0.60 | |
Al+Ti:0.85-1.20 | |||||||||||
Feartan corporra
dùmhlachd | puing leaghaidh | Stàite alloy | neart tensile | neart toraidh | Leudachadh aig àm briseadh |
8.0g / cm³ | 1350-1400 ℃ | Rm N/mm2 | Rp0.2 N/mm2 | A5% | |
800 | ≥550 | ≥241 | ≥25 | ||
810/811 | ≥450 | ≥170 | ≥30 |
GNATH-FHOCAIL
Bathar | Ìre ASTM | Inbhe ASME | Inbhe AMS |
Duilleag, clàr, stiall | B409 | SB409 | 5871 |
pìob & tiùb fuaigheil | B163.B407 | SB163.SB407 | - |
pìob & tiùb tàthaichte | B514 | - | - |
Bàr, cèic | B408 | SB408 | - |
cruthachadh | B564 | SB564 | - |
Iarrtas toraidh
800: 1. Tiùban eileamaid teasachaidh le deagh fheartan meacanaigeach. 2. Sgàineadh fìon-dhearcan le strì an aghaidh corrach aig àm giollachd Airson tagraidhean suas gu 600 ° C tha an alloy air a thoirt seachad ann an staid annealed Airson tagraidhean aig teòthachd àrd tha an alloy air a thoirt seachad ann an staid fuasgladh annealed.
810: 1. Co-dhlùthadair searbhag nitric an aghaidh corrach ann an searbhag nitric. 2. Tiùban teasachaidh smùid feartan meacanaigeach fìor mhath. 3. Heating eileamaid tubes fìor mhath meacanaigeach feartan airson iarrtasan suas ri 500 ° C àrainneachd alloy solair staid airson an annealed staid.