Leave Your Message
Nickel Alloy GH4169/N07718 - Babban Ayyuka na Musamman don Matsanancin Yanayi

Superalloy Series

Nickel Alloy GH4169/N07718, wanda akafi sani da Inconel 718, babban babban aiki ne wanda aka tsara don matsananciyar yanayi. Wannan gawa na nickel-chromium sananne ne don ƙarfinsa na musamman, juriyar lalata, da juriya da iskar shaka a yanayin zafi mai girma. Yana nuna ƙarfin ƙarfin ƙarfi, creep, da rupture ƙarfi, GH4169/N07718 shine manufa don aikace-aikace a cikin sararin samaniya, samar da wutar lantarki, da masana'antar mai da gas. Kyakkyawan weldability ɗin sa da ikon kula da kaddarorin inji a yanayin zafi har zuwa 1300°F (700°C) ya sa ya zama abin dogaro ga mahalli masu buƙata. Ko ana amfani dashi a cikin injin turbin iskar gas, injinan jirgin sama, ko abubuwan haɗin gwiwa, Nickel Alloy GH4169/N07718 yana tabbatar da dorewa da inganci a cikin aikace-aikacen mafi ƙalubale.

    HADIN KASHIN KIMIYYA

    SARKI

    %

    A ciki

    Cr

    Fe

    Domin

    Nb

    Co

    C

    Mn

    Kuma

    S

    Tare da

    Al

    Na

    P

    B

    GH4169
    N07718

    MIN

    50

    17

    daidaitawa

    2.8

    4.75

    -

    -

    -

    -

    -

    -

    0.2

    0.65

    -

    -

    MAX

    55

    21

    daidaitawa

    3.3

    5.5

    1

    0.08

    0.35

    0.35

    0.015

    0.3

    0.8

    1.15

    0.015

    0.06

    Abubuwan Jiki

    yawa

    Aloy state

    karfin jurewa

    samar da ƙarfi

    Tsawaitawa

    Tsawaitawa

     

    N/mm2

    Rp0.2 N/mm2

    A5%

    HB

    8.24g/cm

    Magani mai ƙarfi

    ≥965

    ≥550

    ≥30%

    ≤363

    Magani mai ƙarfi + tsufa

    ≥1275

    ≥1034

    ≥12%

    ≥331

    STANDARD MAI GIRMA

    KYAUTA

    Matsayin ASTM

    Matsayin ASME

    Sheet, Plate, Strip

    B670

    Saukewa: SB670

    Pipe&tube mara kyau

    B983

    -

    welded Pipe&tube

    -

    -

    Bar, Cake

    B637

    Saukewa: SB637

    Ƙirƙira

    B670

    Saukewa: SB670

    Waya

    -

    -

    SIFFOFIN samfur

    1.saukin injina. 2. Ƙarfin ƙarfi mai ƙarfi, ƙarfin gajiya, ƙarfin rarrafe da ƙarfin karaya a 700 ° C. 3. high oxidation juriya a 1000 ° C. 4. barga sinadaran abun da ke ciki a low yanayin zafi. 5. mai kyau weldability.

    Aikace-aikacen samfur

    Saboda da high zafin jiki ƙarfi da kyau kwarai lalata juriya a 700 ℃, sauki aiki 718 za a iya yadu amfani da dama high-buƙata lokatai.

    Nuni samfurin