0102030405
MOTS'EOA CHEMEKE
SEBAKA | % | Ho | Kr | Fe | Bakeng sa | Nb | Co | C | Mong | Le | S | Ka | Al | Ea | P | B |
GH4169 | MIN | 50 | 17 | tekatekano | 2.8 | 4.75 | - | - | - | - | - | - | 0.2 | 0.65 | - | - |
MAX | 55 | 21 | tekatekano | 3.3 | 5.5 | 1 | 0.08 | 0.35 | 0.35 | 0.015 | 0.3 | 0.8 | 1.15 | 0.015 | 0.06 |
Lintho Tsa 'Mele
tekano | Alloy state | matla a tšepe | fana ka matla | Elongation | Elongation |
| Rm N/mm2 | Rp0.2 N/mm2 | A5% | HB | |
8.24g/cm | Kalafo ea tharollo e tiileng | ≥965 | ≥550 | ≥30% | ≤363 |
Tharollo e tiileng + botsofali | ≥1275 | ≥1034 | ≥12% | ≥331 |
TS'ELISO MOEKETSI
PRODUCT | Boemo ba ASTM | Boemo ba ASME |
Leqephe, Letlapa, Lekhapetla | B670 | SB670 |
Seamless Pipe&tube | B983 | - |
weld Pipe&tube | - | - |
Bare, kuku | B637 | SB637 |
Ho qapa | B670 | SB670 |
Mohala | - | - |
Sehlahisoa SEHLOOHO
1. bonolo machinability. 2. matla a phahameng a tsitsipano, matla a mokhathala, matla a ho hahaba le matla a ho robeha ho 700°C. 3. khanyetso e phahameng ea oxidation ho 1000°C. 4. sebopeho sa lik'hemik'hale se tsitsitseng ka mocheso o tlase. 5. weldability e ntle.
Sesebelisoa sa sehlahisoa
Ka lebaka la matla a mocheso o phahameng le khanyetso e ntle ea kutu ho 700 ℃, ts'ebetso e bonolo ea 718 e ka sebelisoa haholo liketsahalong tse fapaneng tse hlokang haholo.