NAFASI | % | Katika | Cr | Fe | Kwa | Nb | Co | C | Mhe | Na | S | Na | Al | Ya | P | B |
GH4169 | MIN | 50 | 17 | usawa | 2.8 | 4.75 | - | - | - | - | - | - | 0.2 | 0.65 | - | - |
MAX | 55 | 21 | usawa | 3.3 | 5.5 | 1 | 0.08 | 0.35 | 0.35 | 0.015 | 0.3 | 0.8 | 1.15 | 0.015 | 0.06 |
Sifa za Kimwili
msongamano | Hali ya aloi | nguvu ya mkazo | kutoa nguvu | Kurefusha | Kurefusha |
| Rm N/mm2 | Rp0.2 N/mm2 | A5% | HB | |
8.24g/cm | Matibabu ya suluhisho thabiti | ≥965 | ≥550 | ≥30% | ≤363 |
Suluhisho thabiti + kuzeeka | ≥1275 | ≥1034 | ≥12% | ≥331 |
KIWANGO CHA MTENDAJI
PRODUCT | Kiwango cha ASTM | Kiwango cha ASME |
Karatasi, Bamba, Ukanda | B670 | SB670 |
Bomba&tube isiyo imefumwa | B983 | - |
svetsade Bomba&tube | - | - |
Baa, Keki | B637 | SB637 |
Kughushi | B670 | SB670 |
Waya | - | - |
Kipengele cha bidhaa
1. rahisi machinability. 2. nguvu ya juu ya mkazo, nguvu ya uchovu, nguvu ya kutambaa na nguvu ya kuvunjika kwa 700°C. 3. upinzani wa juu wa oksidi ifikapo 1000°C. 4. muundo wa kemikali thabiti kwa joto la chini. 5. weldability nzuri.
Maombi ya bidhaa
Kutokana na nguvu ya joto la juu na upinzani bora wa kutu ifikapo 700 ℃, usindikaji rahisi 718 unaweza kutumika sana katika matukio mbalimbali yanayohitaji sana.