KOMPOSISYON NG KEMIKAL
SPACE | % | Sa | Cr | C | Fe | Para sa | SA | Sa | Co | At | Mn | P | S | Nb | Sinabi ni Al | Sa |
HALONG G-30 | MIN | balanse | 28 | _ | 13 | 4 | 1.5 | 1 | _ | 0.2 | 0.3 | _ | _ | 0.3 | _ | _ |
MAX | balanse | 31.5 | 0.03 | 17 | 6 | 4 | 2.4 | 5 | 0.8 | 1.5 | 0.04 | 0.02 | 1.5 | _ | _ | |
HALONG G-35 | MIN | balanse | 32.25 | _ | _ | 7.6 | _ | _ | _ | _ | _ | _ | _ | _ | _ | _ |
MAX | balanse | 34.25 | 0.05 | 2 | 9 | 0.6 | 0.30 | 1 | 0.6 | 0.5 | 0.03 | 0.015 | _ | 0.4 | 0.2 |
Mga Katangiang Pisikal
modelo | densidad | punto ng pagkatunaw | Estado ng haluang metal | lakas ng makunat | lakas ng ani | Pagpahaba sa break | Katigasan ng Brinell |
Rp0.2 N/mm2 | A5% | A5% | HRB | ||||
HALONG G-30 | 8.22g/cm³ | 1350-1370 ℃ | Sheet, plato, strip | ≥586 | ≥241 | ≥30 | _ |
HALONG G-35 | 8.18g/cm³ | 1332-1361 ℃ | 980°C solid solution Paggamot | ≥630 | ≥285 | ≥48 | 80 |
EXECUTIVE STANDARD
produkto | HALONG G-30 | HALONG G-35 |
bar | ASTM B572 | ASTM B574 |
sheet | ASTM B435 | ASTM B575 |
walang tahi na tubo at tubo | ASTM B622 | ASTM B622 |
welded pipe at tubo | ASTM B619 | ASTM B629 |
walang tahi na tubo at tubo | ASTM B626 | _ |
pagpapanday | ASTM B575 | ASTM B472. |
Welding nominal pipe | _ | ASTM B619 |
mga konektor | _ | B366 |