HANA KEMIIKA
KAHIKI | % | In | Cr | ʻO Fe | No ka mea | Nb | ʻO Co | C | ʻO Mn | A | S | Me ka | Ua ʻōlelo ʻo Al | O | P | B |
GH4169 | MIN | 50 | 17 | kaulike | 2.8 | 4.75 | - | - | - | - | - | - | 0.2 | 0.65 | - | - |
MAX | 55 | 21 | kaulike | 3.3 | 5.5 | 1 | 0.08 | 0.35 | 0.35 | 0.015 | 0.3 | 0.8 | 1.15 | 0.015 | 0.06 |
Na Waiwai Kino
mānoanoa | Kūlana huila | ikaika tensile | hāʻawi i ka ikaika | ʻO ka lōʻihi | ʻO ka lōʻihi |
| Rm N/mm2 | Rp0.2 N/mm2 | A5% | HB | |
8.24g/cm | Lapaʻau hoʻonā paʻa | ≥965 | ≥550 | ≥30% | ≤363 |
Paʻa paʻa + ʻelemakule | ≥1275 | ≥1034 | ≥12% | ≥331 |
KUMU HOOKO
HANA | ASTM maʻamau | ASME maʻamau |
Pepa, Papa, Kaha | B670 | SB670 |
Paipu & paipu ʻole | B983 | - |
welded Pipe&tube | - | - |
Bar, Keke | B637 | SB637 |
Ke kalaiwa ana | B670 | SB670 |
Uea | - | - |
HUAKAA HIʻO
1.easy machinability. 2. ka ikaika tensile kiʻekiʻe, ka ikaika luhi, ka ikaika kolo a me ka ikaika haʻihaʻi ma 700 ° C. 3. kiʻekiʻe oxidation kū'ē ma 1000 ° C. 4. paʻa paʻa kemika i nā mahana haʻahaʻa. 5. maikaʻi weldability.
noi huahana
Ma muli o ka ikaika wela kiʻekiʻe a me ke kūpaʻa corrosion maikaʻi loa ma 700 ℃, hiki ke hoʻohana nui ʻia ka hana maʻalahi 718 i nā ʻano hana kiʻekiʻe.