01
KONPOZISYON CHIMIK
Eraum alyaj | % | Nan | Kr | Pou | Fe | NAN | Co | C | Mn | Epi | Nan | P | C | AI | Avèk |
ALOYY C-276 | MIN | kousen | 145 | 15 | 4 | 3 | - | - | - | - | - | - | - | - | - |
MAX | kousen | 16.5 | 17 | 7 | 4.5 | 25 | 0.08 | 1 | 1 | 0.35 | 0.04 | 0.03 | - | ||
ALLOYC-2000 | MIN | kousen | 22 | 15 | - | - | - | - | - | - | - | - | - | - | 1.3 |
MAX | kousen | 24 | 17 | 3 | - | 2 | 0.01 | 0.5 | 0.08 | - | 0.025 | 0.01 | 0.5 | 1.9 |
PWOPRIYETE FIZIK
Modèl | Dansite | Pwen k ap fonn | Fòs rupture | Sede fòs | Elongasyon |
Rm N/mm | RpN/mm | A5% | |||
ALOYY C-276 | 8.9g/cm3 | 1325-1370C | z690 | z283 | z40 |
ALOYY C-2000 | 8.5g/cm3 | 1325-1380C | ≥690 | ≥ 283 | ≥40 |
Egzekitif STANDARD
Pwodwi yo | ALLOYC-276 | ALOYY C-2000 |
Fèy, plak, retire rad sou ou | ASTMB575 | ASTM B575 |
Tib san pwoblèm | ASTMB622 | ASTM B622 |
Tib soude | ASTM B619ASTM B626 | ASTM B619.ASTM B626. |
Ba ak gato | ASTMB574 | ASTM B574 |
Fòje | ASTMB564 | ASTM B564 |
Karakteristik pwodwi
ALLOY C-276 gen ekselan rezistans korozyon, bon machinability ak soudabilite, pa fasil oksidasyon, bon pèfòmans tanperati ki wo, ka kenbe tèt ak kondisyon ekstrèm nan tanperati ki wo ak anviwònman presyon ki wo.
ALLOY C-2000 gen ekselan rezistans korozyon, espesyalman nan rezistans nan korozyon asid silfirik, gen yon trè bon pèfòmans tanperati ki wo ak severite tanperati ki ba, gen yon trè bon rezistans oksidasyon ak rezistans ranpe, segondè fòs, segondè dite, segondè rezistans mete ak lòt pwopriyete mekanik.