N06044
NKWUKWU kemikal
Oghere | % | N'ime | Cr | Fe | Maka | Na | C | Mn | S | Al | Nke | P |
N06044 | MIN | Rem | 43.5 | - | 0.80 | - | - | 0.07 | - | - | - | 0.2 |
MAX | Rem | 45.3 | 0.3 | 1.20 | 0.20 | 0.02 | 0.30 | 0.35 | 0.015 | 0.3 | 0.8 |
Njirimara anụ ahụ
njupụta | ike ọdụdọ | nye ike | Ogologo oge | Ogologo oge |
7.98g/cm² | Rm N/mm2 | Rp0.2 N/mm2 | A5% | HRB |
Ngwọta siri ike | ≥690 | ≥310 | ≥30% | ≤100 |
Ọkọlọtọ EXECUTIVE
Ngwaahịa | ọkọlọtọ ASTM | ọkọlọtọ ASME |
Mpempe akwụkwọ, efere, eriri | B575 | SB575 |
Pipe&tube enweghị nkebi | B622 | - |
welded Pipe&tube | - | - |
Ogwe, achicha | B574 | SB574 |
Na-akpụ akpụ | B564 | SB564 |
Waya | - | - |
Njirimara ngwaahịa
1.N06044 nwere ihe ndị na-arụ ọrụ nke ọma, gụnyere ike dị elu, ike siri ike, ezigbo ike na ike ọgwụgwụ.
Ọ nwere ezigbo nguzogide corrosion na ụlọ okpomọkụ ma nwee ike iguzogide mmebi nke ọtụtụ mgbasa ozi na-emebi emebi dị ka acid, alkali na nnu. Karịsịa na acid siri ike, alkali na gburugburu ebe obibi siri ike, nguzogide corrosion ya dị ịrịba ama.
Antioxidant: Alloy nwere ike ịnọgide na-arụ ọrụ antioxidant kwụsiri ike n'okpuru oke okpomọkụ na nrụgide dị elu, ọ dịghịkwa mfe oxidise na corrode.
Ngwa ngwaahịa
Aerospace: A na-eji ya na-emepụta ihe ọkụ ọkụ dị elu, ọkpọkọ uzuoku na-ekpo ọkụ na ihe ndị ọzọ.