N06044
UKWAKHIWA KWAKHEMICAL
ISIKHALA | % | Ku | Cr | Fe | Ngoba | Futhi | C | UMn | S | Al | Kwe | P |
N06044 | MIN | Rem | 43.5 | - | 0.80 | - | - | 0.07 | - | - | - | 0.2 |
MAX | Rem | 45.3 | 0.3 | 1.20 | 0.20 | 0.02 | 0.30 | 0.35 | 0.015 | 0.3 | 0.8 |
Izakhiwo Zomzimba
ukuminyana | amandla aqinile | veza amandla | Ukwelula | Ukwelula |
7.98g/cm² | Rm N/mm2 | I-Rp0.2 N/mm2 | A5% | I-HRB |
Isixazululo esiqinile | ≥690 | ≥310 | ≥30% | ≤100 |
IZINGA LOKUPHEPHA
PRODUCT | I-ASTM ejwayelekile | I-ASME ejwayelekile |
Ishidi, Ipuleti, Umdweshu | B575 | SB575 |
Ipayipi neshubhu engenamthungo | B622 | - |
Ipayipi elishiselwe | - | - |
Ibha, Ikhekhe | B574 | SB574 |
Ukuqamba | B564 | I-SB564 |
Intambo | - | - |
Isici somkhiqizo
I-1.N06044 inezici ezinhle kakhulu zemishini, kufaka phakathi amandla aphezulu, ubulukhuni obuphezulu, ukuqina okuhle nokumelana nokukhathala.
Inokumelana nokugqwala okuhle ekamelweni lokushisa futhi ingamelana nokuguguleka kwemithombo yezindaba eminingi egqwalayo njenge-asidi, i-alkali nosawoti.Ikakhulukazi ku-asidi eqinile, i-alkali nezinye izindawo ezinokhahlo, ukumelana nokugqwala kwayo kuvelele ngokukhethekile.
I-Antioxidant: I-alloy ingagcina ukusebenza okuzinzile kwe-antioxidant ngaphansi kwezinga lokushisa eliphezulu kanye nokucindezela okuphezulu, futhi akulula uku-oxidise nokugqwala.
Isicelo somkhiqizo
I-Aerospace: Isetshenziselwa ukwakhiwa kwezishisi ezishisa kakhulu, amapayipi esitimu anezinga lokushisa eliphezulu nezinye izakhi.