N06044
HANA KEMIIKA
KAHIKI | % | In | Cr | ʻO Fe | No ka mea | A | C | ʻO Mn | S | Ua ʻōlelo ʻo Al | O | P |
N06044 | MIN | Ua haʻi aku ʻo Rem | 43.5 | - | 0.80 | - | - | 0.07 | - | - | - | 0.2 |
MAX | Ua haʻi aku ʻo Rem | 45.3 | 0.3 | 1.20 | 0.20 | 0.02 | 0.30 | 0.35 | 0.015 | 0.3 | 0.8 |
Na Waiwai Kino
mānoanoa | ikaika tensile | hāʻawi i ka ikaika | ʻO ka lōʻihi | ʻO ka lōʻihi |
7.98g/cm² | Rm N/mm2 | Rp0.2 N/mm2 | A5% | HRB |
Paʻa paʻa | ≥690 | ≥310 | ≥30% | ≤100 |
KUMU HOOKO
HANA | ASTM maʻamau | ASME maʻamau |
Pepa, Papa, Kaha | B575 | SB575 |
Paipu & paipu ʻole | B622 | - |
welded Pipe&tube | - | - |
Bar, Keke | B574 | SB574 |
Ke kalaiwa ana | B564 | SB564 |
Uea | - | - |
HUAKAA HIʻO
1.N06044 maikaʻi nā waiwai mechanical, me ka ikaika kiʻekiʻe, ka paʻakikī kiʻekiʻe, ka paʻakikī maikaʻi a me ke kūpaʻa luhi.
Loaʻa iā ia ke kūpaʻa corrosion maikaʻi ma ka lumi wela a hiki ke kū i ka ʻino o nā media corrosive he nui e like me ka waikawa, ka alkali a me ka paʻakai.
Antioxidant: Hiki i ka alloy ke mālama i ka hana antioxidant paʻa ma lalo o ke kiʻekiʻe kiʻekiʻe a me ke kaomi kiʻekiʻe, a ʻaʻole maʻalahi i ka oxidise a corrode.
noi huahana
Aerospace: Hoʻohana ʻia i ka hana ʻana i nā mea puhi wela wela, nā paipu mahu a me nā mea ʻē aʻe.