0102030405
UKWAKHIWA KWAKHEMICAL
ISIKHALA | % | C | Cr | Ku | Co | Al | Kwe | Fe | Nb | B | Futhi | UMn | S | P | Nge |
GH907 | MIN | - | - | 35.0 | 12.0 | - | 1.3 | ibhalansi | 4.30 | - | 0.07 | - | - | - | - |
MAX | 0.06 | 1.00 | 40.0 | 16.0 | 0.20 | 1.8 | ibhalansi | 5.20 | 0.012 | 0.35 | 1.00 | 0.015 | 0.015 | 0.500 |
Izakhiwo Zomzimba
ukuminyana | Ibanga lokushisa elincibilikayo |
8.28g/cm3 | 1332-1400 ℃ |
Isici somkhiqizo
I-GH907 iyimvula ye-Fe-Ni-Co eyenza lukhuni ukunwebeka okuphansi kwengxube yezinga lokushisa eliphezulu, iqiniswe nge-niobium, i-titanium, i-silicon kanye ne-trace boron. I-alloy inamandla aphezulu, i-coefficient ephansi yokwandisa, ukumelana kahle nokukhathala okushisayo nokubanda kanye ne-modulus ecishe ibe njalo yokunwebeka ngaphansi kuka-650 ℃. Iphoyinti le-Curie liphakathi kuka-400 ℃ no-450 ℃. I-coefficient yokunwetshwa kwe-alloy empeleni ayishintshile ngaphansi kwephoyinti le-Curie. Ingxubevange ilungele ukukhiqizwa kwazo zonke izinhlobo zamasongo enjini yendiza kanye nomagazini ngaphansi kuka-650 ℃, futhi imikhiqizo eyinhloko ihlanganisa imigoqo, ama-forging, amapuleti namapheshana. Ngenxa yokuthi ingxubevange ayinayo i-chromium, izakhi ze-aluminium, ukumelana nokushisa okuphezulu kwe-oxidation akulungile. Uma isetshenziswa isikhathi eside ngaphezu kuka-700 ℃, kufanele kwamukelwe okokuvikela okufanele. Ingaphezulu lengxubevange lingadutshulwa, futhi ukukhathala okugobayo okujikelezayo kungakhuphuka cishe ngo-18% ngemva kokuchama kwesibhamu.
Isicelo somkhiqizo
Ingxubevange isetshenziswe isesimweni esihle ekukhiqizeni omagazini bangemuva be-aero-injini yokucindezela okuphezulu kwe-compressor, izindandatho ezithwala imithwalo, izindandatho ezivikela ukushisa, izindandatho zokuvalwa kwegumbi elivuthayo, izihlalo zekhekheba lezinyosi nezindandatho zangaphandle ze-turbine.