SARKI | % | C | Cr | A ciki | Co | Al | Na | Fe | Nb | B | Kuma | Mn | S | P | Tare da |
GH907 | MIN | - | - | 35.0 | 12.0 | - | 1.3 | daidaitawa | 4.30 | - | 0.07 | - | - | - | - |
MAX | 0.06 | 1.00 | 40.0 | 16.0 | 0.20 | 1.8 | daidaitawa | 5.20 | 0.012 | 0.35 | 1.00 | 0.015 | 0.015 | 0.500 |
Abubuwan Jiki
yawa | Narkewar zafin jiki |
8.28g/cm 3 | 1332-1400 ℃ |
SIFFOFIN samfur
GH907 wani hazo ne na Fe-Ni-Co yana taurare ƙananan nakasar nakasar babban zafin jiki, ƙarfafawa da niobium, titanium, silicon da boron. The gami yana da babban ƙarfi, low coefficient na fadada, mai kyau jure zafi da sanyi gajiya da kusan m modulus na elasticity kasa 650 ℃. Matsayin Curie yana tsakanin 400 ℃ da 450 ℃. Ƙididdiga na faɗaɗa gami da gaske baya canzawa a ƙasan ma'anar Curie. The gami dace da samar da kowane irin jirgin sama da Aerospace engine zobe da mujallu a kasa 650 ℃, da kuma manyan kayayyakin sun hada da sanduna, forgings, faranti da tube. Saboda gami ba ya ƙunshi chromium, abubuwan aluminum, juriya na iskar shaka mai zafi ba shi da kyau. Lokacin amfani da dogon lokaci sama da 700 ℃, ya kamata a yi amfani da kayan kariya masu dacewa. Za a iya harbi saman gami da peened, da jujjuya gajiyar lankwasawa za a iya ƙara da kusan 18% bayan harbi peening.
Aikace-aikacen samfur
An yi amfani da gami a cikin yanayi mai kyau wajen kera mujallu na baya-bayan nan na injin injin mai ɗaukar nauyi, zobba masu ɗaukar nauyi, zoben da ke hana zafi, zoben rufe ɗakin konewa, kujerun saƙar zuma da zoben waje na turbine.